China Spinneret for Chemical Fiber Spinning - High-Quality Suppliers and Factory Solutions
Hot Products

China Spinneret for Chemical Fiber Spinning - High-Quality Suppliers and Factory Solutions

,

The spinneret is an essential component in the manufacturing of synthetic fibers, significantly impacting the fiber spinning process. Typically constructed from high-performance materials such as stainless steel or specialized alloys, a spinneret features numerous tiny holes that allow for the extrusion of polymer melt. Each hole corresponds to a single filament, enabling the simultaneous production of multiple fibers.

,

In the spinning process, the polymer is heated to a molten state and then extruded through the spinneret under controlled pressure. As the molten polymer exits, it cools and solidifies, creating continuous filaments. The design and specifications of the spinneret, including the size and shape of the holes, play a crucial role in determining the properties of the resulting fibers, such as diameter, strength, and texture.

,

Additionally, spinnerets can be customized to manufacture various types of fibers, including monofilaments, multifilaments, and specialty fibers tailored to unique applications. Regular maintenance and precise fabrication are vital for ensuring consistent fiber quality and optimizing production efficiency. As a leading supplier in China, our factory specializes in delivering high-quality spinnerets, empowering the textile industry to mass-produce superior synthetic fibers for diverse applications, from apparel to industrial materials.

,

    Spinneret

    The development and application of synthetic fibers have entered a new stage, with significant variations in fiber types and specifications, and ever-changing processing conditions and parameters. As an indispensable precision component of spinning machines, the spinneret extrudes the spinning melt, which has been precisely measured by the spinning pump, through its micro-holes to form fiber bundles with specific fineness and a dense texture. Its shape and characteristic dimensions are important conditions for ensuring the quality of fiber products.

    SpinneretSpinneret-01

    Material of Spinneret

    The working condition of the spinneret is quite demanding, requiring it to withstand high temperature and pressure while ensuring the quality requirements of the fibers. The material of the spinneret has a significant impact on its mechanical properties and service life. The higher the hardness of the material, the longer the service life of the spinneret, but its processing difficulty will increase.

    ⭐ Therefore, stainless steel with high temperature resistance, corrosion resistance, and excellent mechanical properties should be selected as the material. Commonly used stainless steels include: SUS304, SUS316L, SUS321, SUS431, SUS630, etc.

    Spinneret Classification

    The spinneret is generally classified into Wet Spinning spinneret, Dry Spinning spinneret, and Melt Spinning spinneret.

    1 Wet Spinning Spinneret

    Wet Spinning is one of the major synthetic fiber spinning methods. Firstly the polymers need to be dissolved into solvent. Then the polymer solvent is extruded through the spinneret immersed in tanks which contains the polymer solvent, and then form the filament via solidification. Acrylic, vinyl, rayon are produced by this method.

    In addition, wet spinning is also used to produce carbon fiber. Carbon fiber can be classified into PAN-base, and pitch-base. Nowadays, more than 90% carbon fiber is PAN carbon fiber. The PAN carbon fiber is produced via carbonization procedure of PAN, which is of high tension strength and high elastic strength. In general, wet spinning and dry-wet spinning are the main wet spinning methods. Especially the wet spinning is mostly used, which is of high productivity. In comparison with dry-wet spinning, the spinnerets used for wet spinning have more holes.

    Material Stainless steel, tantalum, gold-platinum alloy
    Number of Holes 200,000, etc.
    Shape Round, rectangular, ring, etc.
    Diameter 0.03–0.3mm or on request
    L/D 1–3 or on request
    Application Rayon, Carbon fiber, Acrylic, Aramid, Vinylon, etc.
    2 Dry Spinning Spinneret

    In dry spinning, the polymer is first dissolved into solvent, then extruded from the spinneret into the hot air and at last solidified into filament due to rapid evaporation. Acetate, acrylic and spandex can be produced in this method. In comparison with round hole spinnerets, the irregular hole spinnerets place higher requirement in the accuracy for the hole of width, length and the angle of guide hole.

    Material Stainless steel, tantalum
    Number of Holes 5,000, etc.
    Shape Round, triangular, etc.
    Diameter 0.06–0.5mm or on request
    L/D 1–15 or on request
    Application Acrylic, Acetate, Triacetate, Spandex, etc.
    3 Melt Spinning Spinneret

    Melt Spinning is one of the major synthetic fiber spinning methods. Its main features are high winder speed, solvent not needed, simple machines and short procedures. Compared with other spinning methods, melt spinning is of high productivity. Melt spinning is mainly used to produce polyester, nylon and PP.

    Material Stainless steel
    Number of Holes On request
    Shape Round, irregular
    Application Polyester, Nylon, PP, staple fiber, etc.

    Spinneret Structure

    1 Spinneret Shape

    The commonly used shape of the spinneret is circular. To be suitable for different types of chemical fiber spinning applications, circular structures are divided into flat plate type, flat plate ring type, and flange flat plate type. There are also rectangular spinnerets, which are divided into flange rectangles, flange groove rectangles, etc.

    2 Spinneret Parameters of Micro Holes

    The diameter of micropores should generally be larger as the viscosity of the melt increases. The viscosity of the following polymers, in descending order, is polyamide, polyester, and polypropylene. The pore diameters of the three spinnerets should be polyamide, polyester, and polypropylene in order from small to large. The micro hole design of the spinning plate should also consider the stretching ratio of the spinning head. After the melt is extruded from the micro holes of the spinning plate, due to the speed difference between the spinning speed and the coiling speed, the fine flow of the melt gradually elongates and becomes thinner in the velocity field along the running direction. The stretching ratio of the spinneret is too small, the stretch of the filament bundle is insufficient, and the strip is uneven, which affects the dyeing performance of the product. Excessive stretching of the spinneret can cause single filament breakage.

    3 Micro Pore Aspect Ratio

    According to the analysis of the flow characteristics of the melt in micropores, increasing the aspect ratio helps with elastic relaxation, reduces the pressure and puffing at the outlet, and makes spinning relatively stable. Principles for selecting aspect ratio:

    1. The residence time of the melt in the pore must be greater than the relaxation time of the melt.
    2. The processability and cleaning conditions of the spinneret must be considered.
    4 Manufacturing Accuracy of Guide Holes and Micropores

    The following are examples of typical specific capillary shapes. Various types of capillary shape produce various characteristics of yarn. It is possible to produce various kinds of specialty yarn by combining polymer kind and spinning condition. Besides these, we can design and produce other shapes. For more details, please contact us.

    Spinneret structure

    Technical Specification

    📐 Surface Roughness of Spinnerets
    Surface Roughness of Spinnerets (ISO) Surface Roughness of Exit Side (ISO)
    Counter sink N5 – N7 Mirror Finish by Polishing N1
    Counter bore N3 – N6 Mat Finish by Lapping N2 – N4
    Transition Angle N2 – N6    
    Capillary N1 – N3    
    🔵 Round Hole Spinnerets
    Dia Of Capillary Length of Capillary Tolerance of Dia Tolerance of Length
    D L/D (≤) Special (±) Precision (±) Special (±) Precision (±)
    φ0.04 – φ0.10 1.00 0.001 0.002 0.001 0.002
    φ0.11 – φ0.20 3.00 0.001 0.002 0.001 0.002
    φ0.21 – φ0.50 5.00 0.001 0.002 0.001 0.002
    φ0.51 – φ1.00 8.00 0.001 0.004 0.002 0.004
    🔷 Profiled Hole Spinnerets
    Width of Slit Length Of Capillary Tolerance Of W Tolerance l.r.d.g.q Tolerance Of L
    W L/D (≤) Special (±) Precision (±) Special (±) Precision (±) Special (±) Precision (±)
    0.04 – 0.06 2.0 0.002 0.003 0.015 0.025 0.02 0.03
    0.06 – 0.10 10.0 0.002 0.003 0.015 0.025 0.02 0.03
    0.10 – 0.20 20.0 0.002 0.003 0.015 0.025 0.02 0.03
    ≥0.20 30.0 0.002 0.003 0.015 0.025 0.02 0.03

    Arrangement of Nozzle Holes

    🔹 5 main arrangement methods: Concentric circle, Square, Diamond, Straight line, Evenly distributed partition, etc.

    Frequently Asked Questions

    Q What is a spinneret and what is its function in fiber production?
    A spinneret is a precision component used in spinning machines. It extrudes the spinning melt — precisely measured by the spinning pump — through its micro-holes to form fiber bundles with specific fineness and a dense texture. Its shape and characteristic dimensions are critical to ensuring the quality of fiber products.
    Q What materials are used to manufacture spinnerets?
    Spinnerets are primarily made from stainless steel due to its high temperature resistance, corrosion resistance, and excellent mechanical properties. Commonly used grades include SUS304, SUS316L, SUS321, SUS431, and SUS630. For wet spinning, tantalum and gold-platinum alloys may also be used.
    Q What are the three main types of spinnerets?
    The three main types of spinnerets are: Wet Spinning Spinnerets (used for rayon, carbon fiber, acrylic, aramid, vinylon), Dry Spinning Spinnerets (used for acrylic, acetate, triacetate, spandex), and Melt Spinning Spinnerets (used for polyester, nylon, PP, and staple fiber).
    Q How does the micro-hole diameter affect spinneret performance?
    The diameter of micropores should generally increase as the viscosity of the melt increases. The pore diameter selection also depends on the stretching ratio: if the stretching ratio is too small, filament strips become uneven and dyeing performance is affected; if it is too large, single filament breakage can occur. Proper micro-hole design is essential for stable spinning and consistent fiber quality.
    Q What are the common shapes of spinneret capillary holes?
    Spinneret capillary holes can be round (most common), triangular, rectangular, irregular/profiled, and other custom shapes. Different capillary shapes produce different yarn characteristics, enabling the production of specialty fibers by combining various polymer types and spinning conditions.
    Q What are the main nozzle hole arrangement methods used in spinnerets?
    There are five main nozzle hole arrangement methods: concentric circle, square, diamond, straight line, and evenly distributed partition. The choice of arrangement affects the uniformity of fiber extrusion and overall spinning efficiency.